본문 바로가기
Guides

POM vs. MC Nylon vs. PEEK for Machined Parts

MaterialsCNC machiningMaterialsNov 9, 2026

Engineering plastic machining means cutting bar and plate stock of mechanical-grade plastics such as POM (acetal), MC nylon, and PEEK into parts the same way as metal. The reason to switch a metal part to plastic is usually one of weight, noise, friction, or electrical insulation, and when ordering you write the material name instead of "plastic". The three commonly used materials differ greatly in moisture absorption and service temperature, so choose the material on those two conditions; the tolerances and measurement conditions you put on the drawing also depend on the material.

Types and Characteristics

POM (Acetal)

POM has low water absorption, so its dimensions are stable, and it has good sliding properties and machinability, which makes it suitable for small room-temperature parts such as gears, cams, and slide blocks. Continuous service temperature is about 80 to 100℃ depending on supplier and grade. Homopolymer (Delrin type) tends to develop porosity at the center of extruded bar, and liquids seep into that porosity, so many suppliers recommend copolymer (POM-C) for food- or fluid-contact parts.

MC Nylon

MC nylon is cast nylon (PA6), made by pouring monomer into a mold and curing it. It is easy to make in large bar and plate sizes, which favors large parts, and it is tough and resistant to impact and wear, so it is mainly used for guide rails, rollers, bushings, and liners. However, it absorbs a lot of moisture: when saturated by soaking in water it absorbs about 6 to 7% by weight, and suppliers advise that in high-humidity environments dimensions can change by up to 2%.

PEEK

PEEK is a high-heat-resistance material with a continuous service temperature of about 250℃, more than double that of POM and MC nylon, and a low saturated water absorption of about 0.5%. Its high stiffness produces few burrs, which favors precision machining, but above the glass transition temperature (Tg, about 143℃) stiffness drops and the coefficient of thermal expansion increases. The material price is generally much higher than POM or MC nylon, so select it only for parts whose temperature and chemical conditions require it.

Teflon (PTFE)

PTFE (Teflon) has a low coefficient of friction and high chemical resistance and heat resistance (about 260℃ continuous). However, it is soft and slowly changes shape under load (creep), and around 19℃ its crystal structure changes, changing volume by about 1%, so avoid it for precision-dimension parts and use it where friction and chemical resistance matter more than dimensions, such as packings, seals, and sliding pads.

Property Comparison

ItemPOMMC NylonPEEKPTFE
Continuous service temperatureAbout 80 to 100℃About 100℃About 250℃About 260℃
Water absorptionLow (0.25% in 24 hours)High (6 to 7% saturated)Low (0.5% saturated)Almost none
Coefficient of linear expansion (×10⁻⁶/℃)About 120About 80About 47 (below Tg)About 160
Wear and impact resistanceGoodVery goodVery goodWeak (creep)
Dimensional stabilityGoodPoor (affected by humidity)Very goodPoor
Relative material costLowLowVery highMedium

The values in the table are typical values from supplier datasheets and vary by grade and test method; for comparison, the coefficient of linear expansion of aluminum is about 23×10⁻⁶/℃.

Applications

PartFirst choiceRationale
Small gears and camsPOMSliding properties, dimensional stability, meshing accuracy
Bushings and slide bearingsPOM or MC nylonPOM for dry environments and small sizes; MC nylon for large sizes and impact
Guide rails, rollers, linersMC nylonLarge stock easy to source, wear resistance
Insulating blocks and fixture supportsPOMMore dimensionally stable than MC nylon
High-temperature areas, steam, chemical contactPEEK250℃ heat resistance, low water absorption
Seals, packings, sliding padsPTFELow friction, chemical resistance

To compare machined stock with 3D printing materials at the prototype stage, see Prototype Material Selection.

Machining Precautions

  • Thermal expansion. POM expands about 5 times more than aluminum: a 100 mm part changes about 0.12 mm in POM and about 0.02 mm in aluminum for a 10℃ temperature change, so measurements differ between the warm state right after machining and at inspection room temperature.
  • Moisture absorption. MC nylon absorbs moisture during storage and use after machining and grows in size, so a dimension that was within tolerance at delivery can go out of tolerance in the field.
  • Residual stress and distortion. Bar and plate stock retain forming stress, so removing a lot of material from one side releases the stress and the part warps. This is especially severe in thin plates and asymmetric pockets, which is why a stress-relief step is sometimes inserted after roughing.
  • Burrs. Tough nylon and soft PTFE form burrs easily, left as long strands along edges, whereas stiff PEEK and POM produce few burrs.
  • Clamping distortion. If a part is machined while clamped tightly, the shape springs back when released and dimensions shift.

If you carry over metal drawing tolerance grades unchanged, dimensions held during machining can fall outside tolerance under inspection conditions. For tolerance values by IT grade see Tolerance Chart Complete Guide, and for the standard that applies to dimensions with no tolerance given see General Tolerances ISO 2768.

Drawing and Purchase Order Notation

  • Material grade. Specify down to the grade, such as "POM-C (acetal copolymer) white", "MC nylon (PA6 cast)", or "PEEK unfilled"; glass-fiber-filled grades have very different properties, so state them separately.
  • Functional dimension tolerances. Even within the same grade, plastic holds tolerance less well than metal, so give individual tolerances only to meshing and bearing-fit areas and leave the rest to general tolerances.
  • Measurement conditions. If there are precision dimensions, write "measured at 20℃", and for MC nylon also state the moisture condition (dry, or after conditioning).
  • Service conditions. Write the service temperature, whether there is water or chemical contact, and whether there is food contact in the notes field or the order memo; the manufacturer uses these conditions to consider alternative materials.

Frequently Asked Questions

How do I choose between POM and MC nylon?

The criteria are humidity and part size. Use POM, with its low water absorption, for parts exposed to water or moisture or where dimensional accuracy matters, and MC nylon for large parts with heavy impact and wear.

Can plastic parts be given the same tolerances as metal?

As dimensions right after machining, yes, but thermal expansion and moisture absorption make dimensions vary with measurement conditions, so apply tolerances only to functional areas and state the measurement conditions with them.

When is PEEK needed?

For parts with a continuous service temperature above 100℃ and parts that contact steam or chemicals; for most room-temperature mechanical parts, POM is enough.

Summary

  • Use POM for room-temperature precision parts, MC nylon for heavily worn parts, and PEEK for high temperature and chemicals.
  • MC nylon changes size with moisture absorption, so consider POM first in water or humid environments.
  • POM, MC nylon, and PEEK have about 2 to 5 times the thermal expansion of aluminum, and warp or twist from residual stress and clamping.
  • Put the material grade, functional dimension tolerances, and measurement conditions on the drawing.

At MakeIT, you request quotes for machined POM, MC nylon, and PEEK parts by uploading a STEP file.

Have a part to machine?

Upload a drawing to see your quote.

Sponsorship & lab support

From competition prep to research projects,
we build alongside student teams and labs.

Questions?

KakaoTalk chat
031-509-0523