Why Anodizing Color Varies from Lot to Lot

FinishingFinishingAug 3, 2026

The Short Answer

Anodizing is not painting. It does not place color on the surface. It converts the aluminum surface into an aluminum oxide film, then adsorbs dye into the film's microscopic pores.

So color depends on these four things.

  1. Alloy composition — With different material, the color differs even under the same conditions.
  2. Coating thickness — The thicker the coating, the more dye it takes in and the darker it gets.
  3. Pretreatment condition — A machined surface and a blasted surface look different even with the same dyeing.
  4. Dyeing and sealing conditions — Varies with concentration, temperature, time, and dye lot.

Color variation is not poor control by the supplier; it is a characteristic that comes from the structure of the process. It cannot be eliminated completely, and the practical solution is to agree at order time on how much variation is acceptable.

How Color Is Applied

When current is applied to aluminum in an electrolyte, the surface oxidizes and an aluminum oxide (Al₂O₃) film grows. This film has a porous structure with countless fine pores.

Dyeing is the process of infiltrating dye into these pores. Sealing then closes the pores to trap the dye.

An important conclusion follows. The amount of space available for dye determines color depth. A thick coating has deeper pores, takes in more dye, and looks darker. A thin one looks lighter. With paint, thickness and color are unrelated, but with anodizing, thickness is color.

Also, because the film is formed by converting the base metal, it does not peel like paint. This is the biggest advantage of anodizing.

Type II and Type III — Different Thickness Means Different Color

CategoryType II (sulfuric)Type III (hard coat)
Coating thickness5~25µm25~100µm
Coating hardness200~400 HV400~700 HV
ColorAll colors possibleLimited to dark colors
Main useDecorative + basic corrosion and wear resistanceHigh wear resistance, functional
Cost and lead timeStandardHigher cost, longer lead time
The specification is MIL‑PRF‑8625 (formerly MIL‑A-8625); Class 1 is undyed and Class 2 is dyed. In Korea these are commonly called "Type 2 and Type 3," but confirm the notation mapping against the supplier's specification.

Requiring a light color on Type III will not give the desired result. Hard anodizing produces a thick film that is itself a dark gray-brown. It is dark even without dyeing. If you need a light or vivid color, you must choose Type II. If you need both a light color and high wear resistance, you must decide which takes priority.

Four Causes of Color Differences Between Lots

1. Alloy Composition

Even for the same "aluminum," alloying elements change the film's transparency and tint.

  • 6061, 5052 — The film forms uniformly and color reproducibility is best.
  • 7075 — Large color variation. The high zinc content affects the film tint.
  • Cast material (ADC12, etc.) — The high silicon content gives a grayish tone or causes blotches. Not suited to light-color dyeing.

If the material changes, the color changes. If the first lot is made in 6061 and the second in 7075, the same color number gives a different color. For parts where color match matters, fix the alloy.

2. Coating Thickness Variation

As explained above, thickness determines color depth. But coating thickness varies with current density, electrolyte temperature, and processing time. Different lots have slightly different conditions.

Also, thickness can differ by location even within a single part. Corners where current concentrates tend to get thicker coating, and inner surfaces far from the electrode get thinner coating. Variation grows with complex shapes and deep pockets.

3. Pretreatment and Surface Roughness

Degreasing and etching before dyeing change the surface condition. And a rough surface scatters light, so the same dyeing looks different.

  • A surface with machining marks and a bead-blasted surface look different even when dyed the same color.
  • If a single part mixes machined and blasted surfaces, the color difference is noticeable.
  • If cutting conditions change and the surface roughness changes, the color changes with it.

If color match matters, specify the surface condition on the drawing as well. Specifying color alone is not enough.

4. Dyeing and Sealing Conditions

Dye concentration, temperature, and immersion time determine color. The dye itself has slight differences between lots. Sealing conditions also affect the final tint.

The processor controls this area, but complete sameness is hard to guarantee. So for products where color control matters, processing everything in one lot is the surest method.

Easy to Miss — Anodizing Increases Dimensions

This is something you must know, apart from color.

The film grows by consuming base metal, so about half of the total film thickness forms inward from the original surface and the other half outward. As a result, dimensions grow by roughly 50% of the total thickness per surface.

For a 50µm film such as Type III, that is about 25µm per surface, or about 50µm across both sides. For precision fits, this is not negligible.

There are two ways to handle it.

  • Compensate at machining — Machine undersize in advance so the final dimension is reached after anodizing.
  • Masking — Specify masking so fit areas and threads are not anodized. Masking is manual, so it adds labor.

If the drawing gives no instruction, parts are processed at the machined dimensions and the problem shows up at assembly.

What to Specify When Ordering

To reduce color variation, state the following on the drawing or order form.

  1. Alloy — 6061, 5052, etc. Fix it if color match matters.
  2. Type and coating thickness — Type II or III, and the target thickness range.
  3. Color — A color number or color sample. A verbal description ("black") is not enough.
  4. Surface condition — As-machined, or pretreatment such as blasting or brushed (hairline) finish.
  5. Masking areas — Fit areas, threads, grounding surfaces, etc.
  6. Acceptable color variation — How much lot-to-lot difference is allowed.

Exchanging color samples is especially reliable. A widely used practice is to secure an approved sample from the first lot and compare later lots against it.

Common Mistakes

  • Specifying a light color on Type III — The film itself is dark, so it cannot be achieved.
  • Changing alloy between lots — The same color number gives a different color.
  • Not specifying masking for fit areas — Dimensions grow by the film thickness and the parts do not assemble.
  • Not specifying surface finish — Machined and blasted surfaces mix and the color looks different within one part.
  • Requesting anodizing on steel parts — Anodizing is for aluminum only. For steel, consider plating or black oxide.
  • Splitting a large quantity into several lots — If color match matters, processing it all at once is safer.

See Also

Upload your drawing together with the color requirements and MakeIT can quote machining and anodizing together.

Have a part to machine?

Upload a drawing to see your quote.

Sponsorship & lab support

From competition prep to research projects,
we build alongside student teams and labs.

Questions?

KakaoTalk chat
031-509-0523