Die casting injects aluminum, zinc or magnesium alloy melted at 600 to 700 degrees into a precision mold at very high pressure and cools it rapidly to form metal parts in volume. Once the mold is built, the cost per part falls to a fraction (tens of times lower) of CNC machining. However, fine internal pores form during high-speed, high-pressure filling, so heat treatment is practically impossible. Price is set by the mold's thermal-fatigue life, cavity count and the part's projected area (clamping tonnage).
Die Casting
Basics
How it works
The principle is the same as plastic injection molding, but the material is molten metal (aluminum, zinc or magnesium alloy) at 600 to 700 degrees. Molten metal is injected into a precision mold at very high pressure and cooled rapidly to form metal parts in volume.
What sets it apart
CNC machining cuts metal parts one at a time from solid blocks. Die casting pours molten metal into a mold and produces thousands to tens of thousands of near-finished metal parts at a time, which makes it well suited to mass production of metal parts.
Process characteristics
✔ Cost-effective for metal volume production — the upfront mold cost is higher than for injection molding, but once the mold is done, the cost per part is a fraction (tens of times lower) of CNC machining and production is faster.
✔ Thin-walled, complex metal shapes — because molten metal is forced in under high pressure, complex shapes with walls as thin as 1 to 3 mm are possible, and structural features such as ribs and bosses can be formed in one piece.
✔ Drawbacks (internal porosity, no heat treatment) — air is trapped as molten metal is forced in at high speed and pressure, creating fine internal pores (porosity). This makes the process unsuitable for pressure vessels or high-strength structural parts, and heat treatment is practically impossible because the trapped gas expands and blisters the part.
Cost structure
Upfront mold cost (higher than injection molding — the tool steel mold must withstand the heat and pressure of molten metal) + alloy material cost (aluminum, zinc or magnesium) + machine running cost by tonnage (clamping force) + trimming and finishing labor
Key cost drivers
① Mold thermal-fatigue life and cavity count
As 600 to 700 degree molten metal repeatedly enters the mold, heat checks (thermal cracks) accumulate on its surface. Mold life is shorter than for injection molds (typically 50,000 to 100,000 shots), so replacement or repair cost is built into the unit price. More cavities lower the cost per part but raise the upfront mold investment.
② Projected area and clamping force
Molten metal is injected at hundreds of atmospheres, so the mold must be held shut with enormous force. Larger, wider parts need a larger die casting machine (for example 800 t vs 3,000 t), and machine cost rises sharply.
③ Trimming and number of finishing steps
Die-cast parts always have a thin metal fin (flash) along the mold parting line, and a trimming step to remove it is essential. Each added CNC post-process (precision holes, tapped threads and so on) raises the price.
Problem drawings (review advised)
Quotes for small prototype runs
The same logic as injection molding applies. With a mold costing tens of millions of KRW, producing only 100 parts puts each part in the hundreds of thousands of KRW. For small metal prototype runs, CNC machining is more economical.
Thick sections with no coring (ribs)
Molten metal shrinks more and cools more slowly than plastic. Thick sections develop internal shrinkage porosity, which sharply reduces strength. Keep wall thickness uniform throughout and reinforce with ribs.
Drawings with no draft angle
Cooled molten metal grips the mold tightly, so a larger draft angle than for plastic injection (typically 2 to 5 degrees) is needed. Without draft, the part will not release from the mold or comes out with scratched surfaces.
Die Casting FAQ
- Q. What is die casting and how does it work?
- The principle is the same as plastic injection molding, but the material is molten metal (aluminum, zinc or magnesium alloy) at 600 to 700 degrees. Molten metal is injected into a precision mold at very high pressure and cooled rapidly to form metal parts in volume.
- Q. Can die-cast parts be heat treated?
- Practically no. Fine pores are trapped inside as metal is forced in at high speed and pressure, and heat treatment makes them expand and blister the part. The process is also unsuitable for pressure vessels and high-strength structural parts.
- Q. How long does a die casting mold last?
- Repeated contact with 600 to 700 degree molten metal builds up heat checks on the surface, so mold life is typically 50,000 to 100,000 shots, shorter than an injection mold. Replacement and repair costs are built into the unit price.
- Q. Can small prototype runs be die cast?
- Not recommended. With a mold costing tens of millions of KRW, producing only 100 parts puts each part in the hundreds of thousands of KRW. For small metal prototype runs, CNC machining is more economical.
- Q. Why should wall thickness be uniform in die cast designs?
- Molten metal shrinks more and cools more slowly than plastic, so thick sections develop internal shrinkage porosity and lose strength sharply. Keep wall thickness uniform throughout and reinforce with ribs.
Die Casting quote from one drawing
Upload STEP or DWG → instant quote → final quote. Analysis through pricing is automated.
Upload a drawing| TitleDie Casting | Scale1:4 | Unitmm | |
| FormatA4 | Date2026-03-12 | Proj. | Sheet1/1 |
| Dwg No.MAKEIT-MASS-DIECASTING | Thk12 | RevA | |