A heat treatment that exposes low-carbon steel parts to a carbon-gas furnace above 900 degrees for a long time so carbon diffuses into the surface only, then quenches them to harden. The surface is hard while the core stays tough, which is essential for parts such as gears that must withstand friction and impact together. Processing is slow, and areas for later machining need extra masking with anti-carburizing paint.
Carburizing
Basics
How it works
Soft, low-carbon steel parts that deform but do not crack easily are exposed for a long time in a carbon-gas furnace above 900 degrees Celsius. Carbon diffuses deep into the surface only, and the part is then rapidly cooled in water or oil (quenching) to harden the surface.
What sets it apart
Induction hardening electrically heats only the surface of medium-carbon steel (S45C, 1045 carbon steel), which is already ready to harden. Carburizing instead "puts steel armor (carbon) on the surface only" of low-carbon steel (such as SCM415) whose core is flexible. It is essential for parts in harsh conditions, such as gear teeth, where the surface must withstand friction and the core must absorb impact.
Process characteristics
✔ A balance of wear resistance and impact resistance — surface hardness becomes much higher than with ordinary heat treatment, while the core, which carbon does not reach, keeps its original toughness, so the part does not shatter under strong impact.
✔ Uniform surface hardening of complex shapes — even narrow corners an induction coil cannot reach and intricately machined 3D shapes are treated, because the gas surrounds the part in the furnace and every surface hardens to a consistent depth.
✔ Drawbacks (long processing time and masking labor) — it takes several hours for carbon to diffuse 1 mm into the material. Areas that will later be drilled or tapped also need anti-carburizing paint applied and dried by hand.
Carburizing FAQ
- Q. How is carburizing different from induction hardening?
- Induction hardening electrically heats only the surface of medium-carbon steel (S45C), which is already ready to harden. Carburizing diffuses carbon into the surface only of low-carbon steel (such as SCM415) whose core is flexible, putting steel armor on the outside.
- Q. What parts need carburizing?
- It is essential for parts in harsh conditions, such as gear teeth, where the surface must withstand friction and the core must absorb impact.
- Q. Do carburized parts resist cracking?
- Surface hardness becomes much higher than with ordinary heat treatment, but the core, which carbon does not reach, keeps its original toughness, so the part does not shatter under strong impact.
- Q. Can complex shapes be carburized uniformly?
- Yes. Even narrow corners an induction coil cannot reach and complex 3D shapes are treated, because the gas surrounds the part in the furnace and every surface hardens to a consistent depth.
- Q. What are the drawbacks of carburizing?
- Processing time is long, since it takes several hours for carbon to diffuse 1 mm into the material. Areas that will later be drilled or tapped also need anti-carburizing paint applied and dried by hand.
Carburizing quote from one drawing
Upload STEP or DWG → instant quote → final quote. Analysis through pricing is automated.
Upload a drawing| TitleCarburizing | Scale1:4 | Unitmm | |
| FormatA4 | Date2026-03-12 | Proj. | Sheet1/1 |
| Dwg No.MAKEIT-POST-CARBURIZING | Thk12 | RevA | |