본문 바로가기
Guides

Why SUS430 (430 Stainless) Costs Half of 304

MaterialsMaterialsAug 7, 2026

The Short Answer

  • A magnet sticking to SUS430 (430 stainless steel) is not a defect. It is a characteristic of its crystal structure (ferritic). SUS304 (304 stainless steel) is austenitic and is, in principle, non-magnetic.
  • The main reason for the price gap is nickel. 304 contains at least 8% nickel, while 430 has virtually none. Nickel is the most expensive component in stainless steel cost.
  • The selection rule is simple: 430 for indoor, dry environments where cost matters; 304 where water, detergents, outdoor exposure, or food contact are involved.

Where "Stainless" Splits

Stainless steel is steel with at least 10.5% chromium, which forms a passive film on the surface. Up to this point 430 and 304 are the same. They diverge on nickel.

  • SUS430 (ferritic) — about 16–18% chromium, no nickel. Its crystal structure is in the same family as ordinary iron, so a magnet sticks to it.
  • SUS304 (austenitic) — 18–20% chromium + 8–10.5% nickel. Nickel changes the crystal structure to make it non-magnetic, and raises corrosion resistance, toughness, and formability a step.

So the myth that "magnetic stainless = fake" is wrong. 430 is a standard grade designed that way from the start, and is widely used in volume for refrigerator doors, kitchen panels, and architectural interior finishes.

Why It Is Up to Half the Price

In stainless steel pricing, nickel is the most expensive element and also the most volatile. 304 contains at least 8% nickel, so its material cost tracks the nickel market directly. 430 carries no such burden, so for the same sheet thickness it is clearly cheaper than 304, and its price is relatively stable. As a side effect, 430 is especially economical for large-area panels where price per weight matters.

What You Give Up — Corrosion Resistance

  • 304: Resists atmosphere, fresh water, detergents, and food acids well across the board. That is why it is the default for kitchenware, food equipment, and outdoor parts. (Seawater and chloride environments are a limit even for 304 and belong to 316 → SUS304 vs SUS316)
  • 430: Sufficient in indoor dry environments, but where salt, detergents, or moisture persist, pitting corrosion comes first. Using 430 where water touches, outdoors, or in food contact does not save money; it shortens the replacement cycle.

Differences in Machining

  • Bending and forming: 304 has higher elongation and suits deep forming. 430 bends normally but reaches its limit in severe forming → Sheet Metal Bending Process Details
  • Machining: 304 work-hardens strongly and is sensitive to cutting conditions. 430 is relatively mild.
  • Welding: 304 is generally easier to handle. 430 requires caution in welded structures because of reduced toughness in the weld zone.

Pitfalls of the Magnet Test

"If a magnet sticks it's 430, if not it's 304" is mostly true, but there is a pitfall: areas of 304 that have been heavily cold-worked, such as by bending or pressing, can change partly in structure and become weakly magnetic. A slight magnet attraction at a bend corner is not a reason to suspect material fraud. If material verification really matters, use the mill sheet (test certificate), not a magnet.

Selection Summary

  • Where 430 fits: Indoor equipment panels and covers, appliance exteriors, architectural interior trim — large-area parts in dry locations.
  • Where you need 304: Kitchen and food contact, outdoor use, equipment that is washed repeatedly, welded structures, deep-formed parts.
  • If in doubt, 304 — if you cannot be sure of the environment, choosing 430 leads to regret from corrosion, while choosing 304 costs only a little more. The risk is highly asymmetric.

Common Mistakes

  • "It's stainless, so it won't rust" — When 430 rusts outdoors or in a wet environment, it is mistaken for defective material. It is a grade selection problem.
  • Judging by magnet response alone — Without knowing that cold-worked 304 is weakly magnetic, you end up returning good material.
  • Writing only "SUS" on the drawing — A drawing without a grade gets quoted with a different material by each supplier. Always specify 430/304/316.
  • Specifying 430 for welded structures — If you do not account for the degraded properties of the weld zone, structural reliability suffers.

See Also

Upload a drawing and MakeIT can show you a quote based on SUS304 right away. If you are unsure which grade to choose, leave a note about the operating environment.

Have a part to machine?

Upload a drawing to see your quote.

Sponsorship & lab support

From competition prep to research projects,
we build alongside student teams and labs.

Questions?

KakaoTalk chat