Laser Cutting

Laser Cutting

Laser cutting is the standard sheet metal method: a high-power fiber laser is focused on the sheet to cut it. Being non-contact, it is fast with no tool wear, but it creates a heat-affected zone (HAZ). Price is set by thickness, number of piercings, assist gas (nitrogen or oxygen) and material scrap rate (nesting).

Standard sheet metal laser (fiber laser)

Basic concept

Laser cutting is a sheet metal process that focuses a high-power laser beam on metal or plastic sheet to cut it precisely. A very high-density beam amplified in optical fiber is the most widely used method for cutting outlines and holes in thin sheet such as SS400 (mild steel, similar to ASTM A36), SUS304 (304 stainless steel) and aluminum. The assist gas determines cutting speed and edge quality.

Assist gas - Oxygen (O₂) - for SS400 mild steel, the combustion reaction increases speed (the cut edge turns black)

Nitrogen (N₂) - used for stainless steel and aluminum, and for clean cuts that prevent edge oxidation

Air - a cost-effective option (compressed air)

Fiber lasers have displaced CO2 lasers and are now the standard equipment in Korean sheet metal and fabrication shops.

Process characteristics

✔ Very high cutting speed (incomparable with wire EDM, especially on 1 to 5T thin sheet)

✔ Non-contact process (no tool wear, and the metal is not physically distorted)

✔ Complex geometries and perforation (punching) are easy

✔ A heat-affected zone (HAZ) forms, so take care with later precision work such as tapping or reaming

Cost structure

Material cost (including scrap rate)

Gas consumption (nitrogen > oxygen)

Number of piercings

Material handling (loading and unloading)

Key cost drivers

① Thickness (T) (the main speed factor)

1T steel plate cuts quickly, but above 20T speed drops sharply and a high-power machine (with a higher hourly rate) is required. The thicker the plate, the more steeply the price rises.

② Number of piercings

Starting a cut by piercing a hole in the middle of the plate takes far longer than entering from the plate edge. Drawings with many holes, like a honeycomb, cost more.

③ Assist gas type

Cutting with nitrogen (N2) to prevent oxidation (rust) costs more than oxygen cutting because the gas is more expensive. (Nitrogen cutting is required if painting or plating follows.)

④ Material scrap rate (nesting)

Material cost depends on how efficiently parts are laid out on a full sheet (for example 4x8), which is called nesting.

Problem drawings

Overlapping lines

If lines overlap, the laser travels the same path twice, which can cause distortion or defects.

Splines and open objects

Slightly broken lines or complex curves slow machine processing and greatly increase cutting time.

Holes smaller than the thickness

(For example, a 3 mm diameter hole in 5T plate) Heat builds up and makes cutting difficult. In general, only holes at least 1 to 1.5 times the thickness are recommended for laser cutting.

3D models without a flat pattern

Sheet must be cut flat (2D DXF), so if only a 3D shape is provided, a separate unfolding step is needed at the CAM stage.

Uncleaned text or dimension lines in the drawing

The laser may treat text or dimension lines as cutting targets, causing machining errors.

Laser Cutting FAQ

Q. What is the difference between laser cutting assist gases?
Oxygen (O₂) speeds up cutting of SS400 mild steel through a combustion reaction, but the cut edge turns black. Nitrogen (N₂) is used for stainless steel and aluminum and for clean cuts that prevent edge oxidation, and it costs more than oxygen because the gas is more expensive. Air is used for cost-focused cutting.
Q. What determines the price of laser cutting?
The thicker the plate (T), the more sharply speed drops and the higher the price. More piercings, where a hole is made in the middle of the plate, add cutting time. The assist gas and the material scrap rate from how efficiently parts are nested on a full sheet also affect price.
Q. What is the smallest hole a laser can cut?
In general, only holes at least 1 to 1.5 times the thickness are recommended. Holes smaller than the thickness (for example, a 3 mm diameter hole in 5T plate) are difficult because heat builds up.
Q. Can a laser cut directly from a 3D model alone?
Sheet must be cut flat (2D DXF), so if only a 3D shape is provided without a bend flat pattern, a separate unfolding step is needed at the CAM stage.
Q. What should I watch for when preparing a laser cutting drawing?
Overlapping lines make the laser travel the same path twice, which can cause distortion or defects, and slightly broken splines or complex curves increase cutting time. If text or dimension lines are not cleaned up, the laser may treat them as cutting targets and cause errors.

Laser Cutting quote from one drawing

Upload STEP or DWG → instant quote → final quote. Analysis through pricing is automated.

Upload a drawing
TitleLaser CuttingScale1:4Unitmm
FormatA4Date2026-03-12Proj.Sheet1/1
Dwg No.MAKEIT-LASER-CUTTINGThk12RevA

Related: Sheet fabrication

Sheet fabrication services

Read more