What to Check Before Ordering Titanium Parts

CostCNC machiningMaterialsNov 9, 2026

Titanium machining means cutting commercially pure titanium and titanium alloys (mainly Ti‑6Al‑4V) into parts. Quotes often come out higher than for the same shape in aluminum, and the cause is often machining time and tooling cost rather than the material price. So when ordering, decide the grade first, then compare against substitute materials to judge whether the part truly needs titanium.

Types and standard designations

Most titanium used for machined parts falls into two: Grade 2, commercially pure titanium with no alloying elements, and Grade 5 (Ti‑6Al‑4V), which contains 6% aluminum and 4% vanadium.

ItemGrade 2 (pure titanium)Grade 5 (Ti‑6Al‑4V)
Tensile strength (min, ASTM B348 bar)345 MPa895 MPa
0.2% yield strength (min)275 MPa828 MPa
Corrosion resistanceExcellentExcellent (many sources say slightly lower than Gr2)
MachinabilityRelatively easy, but soft, so chips stickHigher strength causes more tool wear
Main usesChemical equipment, piping, corrosion-resistant partsAerospace, high-strength structural parts, high-load fastening areas

If strength is needed, consider Gr5 first; if corrosion resistance and formability are the goal, consider Gr2. The two grades differ by more than a factor of two in minimum tensile strength and the manufacturer quotes by grade, so the material field on the drawing must state the grade, Gr2 or Gr5.

Machining characteristics

  • Thermal conductivity: The thermal conductivity of Ti‑6Al‑4V is about 6.7 W/m·K, roughly one-twentieth that of aluminum alloys (about 130 to 170 W/m·K), so cutting heat cannot escape and builds up right at the tool edge.
  • Reaction with the tool: At high temperature, titanium tends to weld onto the tool surface, dulling the edge quickly; shorter tool life increases both tooling cost and changeover time.
  • Cutting speed: To reduce heat, spindle speed must be lowered; according to tool manufacturer data, the milling speed for Ti‑6Al‑4V is about 50 to 70 m per minute, far lower than for aluminum, so machining time is longer even for the same shape.
  • Elastic modulus: About half that of steel, so thin walls are pushed away by cutting force and then spring back, causing chatter and dimensional variation.
  • Material supply: The thicknesses and diameters in circulation are fewer than for aluminum or SUS, so sometimes you buy stock larger than the desired size and cut away a lot; in this case both the material unit price and the amount scrapped rise.

In short, titanium is a material where two CNC price factors, "material" and "machining time", grow at the same time; price factors overall are covered in What determines CNC machining price.

Comparison with aluminum and SUS

MaterialTensile strength (MPa)Density (g/cm³)Corrosion resistanceBiocompatibilityMachining difficultyRelative cost
AL6061‑T6 (6061 aluminum)About 3102.70ModerateNot for this useEasyLow
AL7075‑T6 (7075 aluminum)About 5702.81LowNot for this useEasyMedium
SUS316520 or moreAbout 8.0High316L is used for medicalDifficultMedium
Ti Gr2345 or moreAbout 4.5Very highImplant standards existDifficultHigh
Ti Gr5895 or more4.43Very highELI grade is for implantsVery difficultHighest

The aluminum values in the table are typical values, while the SUS and titanium values are standard minimums, so the bases differ. Relative cost is a tendency combining material cost and machining time, and the order can change with shape and quantity.

Judging use and substitute materials

In terms of specific strength (strength divided by weight), the difference between Ti Gr5 and AL7075‑T6 is not large, so if strength-to-weight is the goal, AL7075 is sometimes enough, and machining cost drops substantially. However, if higher strength is needed in the same volume, or the service temperature is in a range aluminum can hardly withstand, use titanium.

If corrosion resistance is the goal, consider SUS316 (316 stainless steel) first. SUS316 handles general chloride environments in many cases. The difference between the two steel grades is covered in SUS304 vs SUS316. Titanium is advantageous where even 316 suffers pitting, such as long-term seawater immersion or oxidizing environments like wet chlorine and nitric acid. However, it is not used in hydrofluoric acid or hot hydrochloric acid environments. In particular, if human implantation or biological contact is a requirement, you must specify titanium that meets the applicable medical standard.

Ordering considerations

  • Standard and grade: State the standard and grade matching the product form, such as ASTM B348 for bar and ASTM B265 for plate; for medical use there are separate standards such as ASTM F67 (pure titanium) and ASTM F136 (Ti‑6Al‑4V ELI).
  • Material certificate (mill sheet): This is the evidence that composition and mechanical properties meet the standard, so request it at the order stage if needed.
  • Tolerance and surface: Applying precision tolerances to thin walls or long overhangs greatly increases machining time, so specifying them only where functionally necessary costs less.
  • Anodized coloring: Unlike aluminum anodizing, titanium anodizing produces color through light interference that depends on oxide film thickness, and the film thickness and color are set by changing voltage. Color can differ with material and pretreatment condition, so agree on a color sample as well; aluminum anodizing is covered in Aluminum surface finish types.

Drawing and purchase order notation

In the material field of the title block, write the grade and standard together; if a mill sheet or anodizing is needed, instruct it separately in a note; general tolerance and surface roughness are noted the same way as for other materials.

ItemNotation example
Material (Gr5)Ti‑6Al‑4V (ASTM B348 Gr5), annealed condition
Material (Gr2)Pure titanium (ASTM B348 Gr2)
Note (mill sheet)Attach material certificate
Note (anodizing)Color, per sample

Frequently asked questions

Should the drawing say whether it is Gr2 or Gr5?

Yes. The two grades differ by more than a factor of two in minimum tensile strength, so with a different grade, even the same shape is a different part.

What conditions change titanium machining cost greatly?

It varies greatly with shape, quantity, and tolerance; the more thin walls and deep pockets, the longer the machining time and the higher the machining cost.

Can titanium parts be colored?

Yes. Anodizing can produce gold, blue, and purple tones, and because the color comes from the oxide film itself, fading is rarely a problem.

Summary

  • The grade is Gr5 for strength and Gr2 for corrosion resistance and formability; when ordering, state the standard, grade, mill sheet, and coloring criteria together.
  • The causes of high machining cost are low thermal conductivity, tool welding, low cutting speed, and material supply.
  • If you only need strength-to-weight, AL7075 is sometimes enough; for general corrosion resistance, SUS316 sometimes suffices.

On MakeIT, you can upload a STEP file and get separate quotes in titanium and in substitute materials to compare.

Have a part to machine?